| Sistēmas prasības |
| A 3D printer with 1.75 mm extruder of temperature around 220 °C. |
| NOTE1: PVA will not dissolve completely and should be easily peeled off by hand. It is recommended to peel it off when the water temperature is between 50–60°C for effortless removal. |
| NOTE2:If the main material is PLA, the water temperature should not exceed 60°C, as higher temperatures may cause damage to the model.
|